Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LOXIAMID PA66 GF25 HS1 04027 - PA66-GF25 - Loxim Industries Limited

Material Data Center offers the following functions for LOXIAMID PA66 GF25 HS1 04027:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Loxiamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesValueUnitTest Standard
ISO Data
Stress at break 115 MPa ISO 527
Strain at break 3 % ISO 527
Flexural modulus, 23°C 6200 MPa ISO 178
Flexural strength 150 MPa ISO 178
Izod notched impact strength, +23°C 8 kJ/m² ISO 180/1A
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 200 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 210 °C ISO 75-1/-2
Other propertiesValueUnitTest Standard
Density 1300 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 280 - 300 °C -
Mold temperature 80 - 90 °C -
Characteristics
Processing
Injection Molding
Delivery form
Black
Additives
Release agent
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Chemical Resistance
General Chemical Resistance
Applications
Automotive, Building Construction, Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.