Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S ECO 776SE BC40 - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S ECO 776SE BC40:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 53 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 40 %
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 4 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2200 MPa ISO 527
Yield stress 47 MPa ISO 527
Yield strain 3.3 % ISO 527
Nominal strain at break 12 % ISO 527
Flexural modulus, 23°C 2000 MPa ISO 178
Flexural strength 65 MPa ISO 178
Charpy impact strength, +23°C 260 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 30 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 4 kJ/m² ISO 179/1eA
Ball indentation hardness 70 MPa ISO 2039-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 96[ann.] °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 101[ann.] °C ISO 75-1/-2
Vicat softening temperature, B 92 °C ISO 306
Coeff. of linear therm. expansion, parallel 95 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning rate, FMVSS, Thickness 1 mm 25[1] mm/min ISO 3795 (FMVSS 302)
Other Standards[S]
Thermal Conductivity, solid state 0.17 W/(m K) DIN 52612-1
1: 2 mm  S: These properties are reported by the producer according standards that are different to our defaults.  ann.: annealed
Other propertiesValueUnitTest Standard
Water absorption 1.65 % Sim. to ISO 62
Humidity absorption 0.35 % Sim. to ISO 62
Density 1070 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation ExtrusionValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 200 - 250 °C -
Characteristics
Processing
Profile Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets
Special Characteristics
High impact or impact modified, U.V. stabilized or stable to weather
Chemical Resistance
General Chemical Resistance
Certifications
Contains renewable resources, ISCC Plus
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.