Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S KR2858G3 - ASA-GF15 - INEOS Styrolution

Material Data Center offers the following functions for Luran® S KR2858G3:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Luran® S KR2858G3 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S KR2858G3 is a 15% glass fiber reinforced ASA grade offering enhanced heat resistance and superior rigidity.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 5 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 6600 MPa ISO 527
Stress at break 110 MPa ISO 527
Strain at break 2.5 % ISO 527
Charpy impact strength, +23°C 28 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 7 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 110 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 115 °C ISO 75-1/-2
Vicat softening temperature, B 115 °C ISO 306
Coeff. of linear therm. expansion, parallel 30 E-6/K ISO 11359-1/-2
Other propertiesValueUnitTest Standard
Water absorption 1.4 % Sim. to ISO 62
Humidity absorption 0.3 % Sim. to ISO 62
Density 1180 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 240 - 280 °C -
Mold temperature 80 - 95 °C -
Diagrams
Viscosity-shear rate , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Shearstress-shear rate , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Stress-strain , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Secant modulus-strain , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Tensile modulus-temperature , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Europe, Near East/Africa
Other text information
Injection molding
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 240 - 280°C

Mold temperature, range: 40 - 95°C

Application examples
Rotor, wind turbine
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.