Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S KR2864C - (ASA+PC) - INEOS Styrolution

Material Data Center offers the following functions for Luran® S KR2864C:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Luran® S KR2864C is a blend of ASA with PC, shows high heat and high impact resistance and long-term property retention. Its UV resistance is not only sufficient for all kind of interior applications – incl. unpainted surfaces in light colors – but also for exterior parts with medium weatherability requirements. Luran® S KR2864C is a high flow grade with a balanced profile.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 25 cm³/10min ISO 1133
Temperature 260 °C -
Load 5 kg -
Thermal conductivity of melt 0.19 W/(m K) -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2600 MPa ISO 527
Yield stress 63 MPa ISO 527
Yield strain 4.6 % ISO 527
Nominal strain at break >50 % ISO 527
Charpy notched impact strength, +23°C 60 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 11 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 105 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 124 °C ISO 75-1/-2
Vicat softening temperature, B 120 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Other propertiesValueUnitTest Standard
Water absorption 0.6 % Sim. to ISO 62
Humidity absorption 0.18 % Sim. to ISO 62
Density 1150 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 - 110 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 260 - 300 °C -
Mold temperature 60 - 90 °C -
Diagrams
Viscosity-shear rate , Luran® S KR2864C, (ASA+PC), INEOS Styrolution
Shearstress-shear rate , Luran® S KR2864C, (ASA+PC), INEOS Styrolution
Dynamic Shear modulus-temperature , Luran® S KR2864C, (ASA+PC), INEOS Styrolution
Stress-strain , Luran® S KR2864C, (ASA+PC), INEOS Styrolution
Secant modulus-strain , Luran® S KR2864C, (ASA+PC), INEOS Styrolution
Specific volume-temperature (pvT) , Luran® S KR2864C, (ASA+PC), INEOS Styrolution
Tensile modulus-temperature , Luran® S KR2864C, (ASA+PC), INEOS Styrolution
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING

Pre-drying, Temperature: 100 - 110°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 260 - 300°C

Mold temperature, range: 60 - 90°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.