Any use of this information falls under the rules of our
disclaimer.
Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt volume-flow rate, MVR |
18 |
cm³/10min |
ISO 1133 |
Temperature |
190 |
°C |
- |
Load |
2.16 |
kg |
- |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Shore A hardness |
88 |
- |
ISO 7619-1 |
Other Standards[S] |
Flexural modulus, 23°C |
27 |
MPa |
ISO 6721-1 |
Flexural modulus |
72 |
MPa |
ISO 6721-1 |
Flexural modulus temperature |
60 |
°C |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Melting temperature, 10°C/min |
160 |
°C |
ISO 11357-1/-3 |
Vicat softening temperature, A |
90 |
°C |
ISO 306 |
Other Standards[S] |
Glass transition temperature, 10°C/min |
-13.6 |
°C |
ISO 6721-1 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard |
Density |
1200 |
kg/m³ |
ISO 1183 |
Bulk density |
457 |
kg/m³ |
- |
3D Data | Value | Unit | Test Standard |
Other Standards[S] |
Tensile strength, flat |
20[1] |
MPa |
DIN 53504 |
Tensile strength, upright |
15[2] |
MPa |
DIN 53504 |
Strain at break, flat |
520[1] |
% |
DIN 53504 |
Strain at break, upright |
500[2] |
% |
DIN 53504 |
1: | XY-direction | 2: | ZX-direction | S: | These properties are reported by the producer according standards that are different to our defaults. |
Characteristics
Processing
Additive Manufacturing, Laser Sintering
Delivery form
Powder, Natural Color
Applications
Sports Equipment
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com