Processing/Physical Characteristics | Value | Unit | Test Standard |
Other Standards[S] |
Melt Flow Index, MFI |
6 |
g/10min |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Mechanical properties | Value | Unit | Test Standard |
Other Standards[S] |
Flexural Modulus |
2392 |
MPa |
|
Flexural Strength |
55.2 |
MPa |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Thermal properties | Value | Unit | Test Standard |
ASTM Data |
Melting Temperature |
210 |
°C |
ASTM D 3418 |
Optical properties | Value | Unit | Test Standard |
ASTM Data |
Gloss |
90[1] |
- |
ASTM D 2457 |
Haze |
2.1 |
% |
ASTM D 1003 |
Other properties | Value | Unit | Test Standard |
Density |
1240 |
kg/m³ |
ASTM D 792 |
Film Properties | Value | Unit | Test Standard |
ASTM Data |
Tensile Modulus, MD |
3310 |
MPa |
ASTM D 882 |
Tensile Strength, MD |
110 |
MPa |
ASTM D 882 |
Elongation at Break, MD |
160 |
% |
ASTM D 882 |
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament
Special Characteristics
High impact or impact modified
Features
Good Adhesion
Certifications
Contains renewable resources
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com