Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of MAGNUM™ 375 HP - ABS - Trinseo

Material Data Center offers the following functions for MAGNUM™ 375 HP:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Magnum datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 2.1 g/10min ISO 1133
Temperature 230 °C -
Load 3.8 kg -
Molding shrinkage, parallel 0.6 % ISO 294-4, 2577
Molding shrinkage, normal 0.6 % ISO 294-4, 2577
ASTM Data
Melt Flow Index, MFI 2.1 g/10min ASTM D 1238
Temperature 230 °C -
Load 3.8 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2330 MPa ISO 527
Yield stress 47 MPa ISO 527
Yield strain 2.9 % ISO 527
Strain at break 3.5 % ISO 527
Flexural modulus, 23°C 2390 MPa ISO 178
Charpy notched impact strength, +23°C 22 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 11 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 25 kJ/m² ISO 180/1A
Izod notched impact strength 10 kJ/m² ISO 180/1A
Temperature -30 °C -
ASTM Data
Tensile Modulus 2303 MPa ASTM D 638
Tensile Strength at Yield 49 MPa ASTM D 638
Elongation at Yield 3.1 % ASTM D 638
Elongation at Break 8.8 % ASTM D 638
Flexural Modulus 2406 MPa ASTM D 790
Flexural Strength 75.8 MPa ASTM D 790
Izod Impact notched, 1/8 in 219 J/m ASTM D 256
Izod Impact notched, Low-Temperature 133 J/m ASTM D 256
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 84 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 98 °C ISO 75-1/-2
ASTM Data
Coefficient of Thermal Expansion, MD 77.4 E-6/K ASTM D 696
Coefficient of Thermal Expansion, TD 95.4 E-6/K ASTM D 696
DTUL @ 66 psi 99.4 °C ASTM D 648
DTUL @ 264 psi 81.7 °C ASTM D 648
Vicat Temperature 103 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 1060 kg/m³ ISO 1183
Density 1060 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 82 - 85 °C -
Pre-drying - Time ≥2 h -
Melt temperature 243 - 271 °C -
Zone 1 238 °C -
Zone 2 249 °C -
Zone 3 254 °C -
Nozzle temperature 249 - 254 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Applications
Automotive
Regional Availability
North America, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.