Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makroblend® UT235 M - (PC+PET)-T15 - Covestro Deutschland AG

Material Data Center offers the following functions for Makroblend® UT235 M:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makroblend datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
  • (PC PET)-blend, 15% mineral filled, easy flow, low coefficient of linear thermal expansion, easy release, injection molding. Molded parts from UT235M having exceptional dimensional stability.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 4500 MPa ISO 527
Stress at break 67 MPa ISO 527
Strain at break 4 % ISO 527
Charpy impact strength, +23°C 85 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 85 kJ/m² ISO 179/1eU
Puncture - maximum force, +23°C 4500 N ISO 6603-2
Puncture energy, +23°C 36 J ISO 6603-2
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 114 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 128 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 45 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 45 E-6/K ISO 11359-1/-2
Other propertiesValueUnitTest Standard
Water absorption 0.4 % Sim. to ISO 62
Humidity absorption 0.2 % Sim. to ISO 62
Density 1340 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 270 °C ISO 294
Injection Molding, mold temperature 70 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 110 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.01 % -
Melt temperature 260 - 280 °C -
Mold temperature 60 - 80 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING
Max. Water content: 0.01 %
Drying temperature: 110 °C
Drying time:
Circulating air drying oven (50 % fresh air) 4-12 h
Fresh air dryer (high speed dryer) 2-4 h
Dry air dryer 2-4 h

PROCESSING
Melt temperature: 260-280 °C
Mold temperature: 60-80 °C

Use open nozzle.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com