Any use of this information falls under the rules of our
disclaimer.
Product Texts
Partially bio-circular grade.
Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt volume-flow rate, MVR |
7 |
cm³/10min |
ISO 1133 |
Temperature |
300 |
°C |
- |
Load |
1.2 |
kg |
- |
Melt flow index, MFI |
7.5 |
g/10min |
ISO 1133 |
Temperature |
300 |
°C |
- |
Load |
1.2 |
kg |
- |
Molding shrinkage, parallel |
0.8 |
% |
ISO 294-4, 2577 |
Molding shrinkage, normal |
0.8 |
% |
ISO 294-4, 2577 |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Tensile Modulus |
2250 |
MPa |
ISO 527 |
Yield stress |
61 |
MPa |
ISO 527 |
Yield strain |
6 |
% |
ISO 527 |
Nominal strain at break |
>50 |
% |
ISO 527 |
Stress at break |
70 |
MPa |
ISO 527 |
Strain at break |
130 |
% |
ISO 527 |
Flexural modulus, 23°C |
2250 |
MPa |
ISO 178 |
Flexural strength |
88 |
MPa |
ISO 178 |
Charpy impact strength, +23°C |
N |
kJ/m² |
ISO 179/1eU |
Charpy impact strength, -30°C |
N |
kJ/m² |
ISO 179/1eU |
Charpy notched impact strength, +23°C, 3mm |
70 |
kJ/m² |
ISO 179/1eA |
Type of failure |
P |
- |
- |
Charpy notched impact strength, -30°C, 3mm |
60 |
kJ/m² |
ISO 179/1eA |
Type of failure |
P(C) |
- |
- |
Izod notched impact strength, +23°C |
65 |
kJ/m² |
ISO 180/1A |
Izod notched impact strength |
30 |
kJ/m² |
ISO 180/1A |
Temperature |
-30 |
°C |
- |
Puncture - maximum force, +23°C |
5200 |
N |
ISO 6603-2 |
Puncture - maximum force, -30°C |
6100 |
N |
ISO 6603-2 |
Puncture energy, +23°C |
55 |
J |
ISO 6603-2 |
Puncture energy, -30°C |
60 |
J |
ISO 6603-2 |
Ball indentation hardness |
108 |
MPa |
ISO 2039-1 |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Glass transition temperature, 10°C/min |
148 |
°C |
ISO 11357-1/-2 |
Temp. of deflection under load, 1.80 MPa |
125 |
°C |
ISO 75-1/-2 |
Temp. of deflection under load, 0.45 MPa |
139 |
°C |
ISO 75-1/-2 |
Vicat softening temperature, B |
146 |
°C |
ISO 306 |
Coeff. of linear therm. expansion, parallel |
70 |
E-6/K |
ISO 11359-1/-2 |
Coeff. of linear therm. expansion, normal |
70 |
E-6/K |
ISO 11359-1/-2 |
Burning behav. at 1.5 mm nom. thickn. |
HB |
class |
IEC 60695-11-10 |
Thickness tested |
1.5 |
mm |
- |
Oxygen index |
30 |
% |
ISO 4589-1/-2 |
Glow Wire Flammability Index (GWFI) |
850 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (1) |
0.75 |
mm |
- |
Glow Wire Flammability Index (GWFI) |
850 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (2) |
1.5 |
mm |
- |
Glow Wire Flammability Index (GWFI) |
900 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (3) |
3 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
800 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (1) |
0.75 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (2) |
1.5 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (3) |
3 |
mm |
- |
Other Standards[S] |
Thermal Conductivity, solid state |
0.2 |
W/(m K) |
ISO 8302 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Electrical properties | Value | Unit | Test Standard |
ISO Data |
Volume resistivity |
1E14 |
Ohm*m |
IEC 62631-3-1 |
Surface resistivity |
1E16 |
Ohm |
IEC 62631-3-2 |
Electric strength |
34 |
kV/mm |
IEC 60243-1 |
Comparative tracking index |
225 |
- |
IEC 60112 |
Other Standards[S] |
Relative permittivity, 100Hz |
3.1 |
- |
IEC 60250 |
Relative permittivity, 1MHz |
3 |
- |
IEC 60250 |
Dissipation factor, 100Hz |
12 |
E-4 |
IEC 60250 |
Dissipation factor, 1MHz |
120 |
E-4 |
IEC 60250 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Optical properties | Value | Unit | Test Standard |
ISO Data |
Luminous transmittance |
89[1] |
% |
ISO 13468-1, -2 |
Other Standards[S] |
Index of Refraction |
1.59 |
- |
ISO 489 |
1: | 2 mm | S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard |
Water absorption |
0.4 |
% |
Sim. to ISO 62 |
Humidity absorption |
0.12 |
% |
Sim. to ISO 62 |
Density |
1200 |
kg/m³ |
ISO 1183 |
Bulk density |
640 |
kg/m³ |
- |
Test specimen production | Value | Unit | Test Standard |
ISO Data |
Injection Molding, melt temperature |
300 |
°C |
ISO 294 |
Injection Molding, mold temperature |
80 |
°C |
ISO 294 |
Injection Molding, injection velocity |
200 |
mm/s |
ISO 294 |
Processing Recommendation Injection Molding | Value | Unit | Test Standard |
Pre-drying - Temperature |
120 |
°C |
- |
Pre-drying - Time |
2 - 3 |
h |
- |
Processing humidity |
≤0.02 |
% |
- |
Melt temperature |
280 - 320 |
°C |
- |
Mold temperature |
80 - 120 |
°C |
- |
Zone 1 |
250 - 260 |
°C |
- |
Zone 2 |
270 - 280 |
°C |
- |
Zone 3 |
280 - 290 |
°C |
- |
Nozzle temperature |
290 - 300 |
°C |
- |
Back pressure |
5 - 15 |
MPa |
- |
Characteristics
Processing
Injection Molding
Special Characteristics
High impact or impact modified
Certifications
Contains renewable resources, Food contact, ISCC Plus
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com