Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® FR6020 RE - PC-I FR(40) - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® FR6020 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
  • polycarbonate
  • medium viscosity
  • easy release
  • UV stabilized
  • flame retardant
  • chlorine- and bromine-free flame retardancy
  • non-reinforced
  • good hydrolysis resistance
  • impact modified
  • Information technology
  • electrical/electronic
Partially bio-circular grade / Attributed via mass balance (according to ISCC PLUS Standard).
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 9 cm³/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
Molding shrinkage, parallel 0.7 % ISO 294-4, 2577
Molding shrinkage, normal 0.7 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2380 MPa ISO 527
Yield stress 58 MPa ISO 527
Yield strain 6 % ISO 527
Flexural modulus, 23°C 2430 MPa ISO 178
Flexural strength 90 MPa ISO 178
Charpy notched impact strength, +23°C 69 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 33 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 67 kJ/m² ISO 180/1A
Izod notched impact strength 26 kJ/m² ISO 180/1A
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 114 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 127 °C ISO 75-1/-2
Vicat softening temperature, B 134 °C ISO 306
Coeff. of linear therm. expansion, parallel 49 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 58 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 2.0 mm -
Burning Behav. 5V at thickness h 5VB class IEC 60695-11-20
Thickness tested 2.0 mm -
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 300 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Melt temperature 280 - 300 °C -
Mold temperature 80 °C -
Characteristics
Processing
Injection Molding
Additives
Release agent
Special Characteristics
Flame retardant, Halogen-free, High impact or impact modified, U.V. stabilized or stable to weather
Chemical Resistance
Hydrolytically Stable
Certifications
Contains renewable resources, ISCC Plus
Applications
Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.