Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Marlex® HXM 50100 - (PE-HD) - Chevron Phillips Chemical Co. LP

Material Data Center offers the following functions for Marlex® HXM 50100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Marlex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 10 g/10min ASTM D 1238
Temperature 190 °C -
Load 21.6 kg -
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 24.8 MPa ASTM D 638
Elongation at Break 700 % ASTM D 638
Flexural Modulus 1207 MPa ASTM D 790
Shore D Hardness 68 - ASTM D 2240
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 78.3 °C ASTM D 648
Vicat Temperature 126 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 948 kg/m³ ASTM D 792
Characteristics
Processing
Blow Molding, Thermoforming
Delivery form
Pellets
Special Characteristics
High impact or impact modified
Features
Melt Strength, Copolymer, Hexene Copolymer
Chemical Resistance
General Chemical Resistance, Environmental Stress Crack Resistance
Certifications
Food contact, Food approval FDA 21 CFR, Drinking water contact, Drinking water contact NSF 61, Drug Master File
Applications
Automotive, Medical, Packaging, Sports Equipment
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.