Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Moplen HP400H - PP - LyondellBasell Industries

Material Data Center offers the following functions for Moplen HP400H:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Moplen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 2 g/10min ISO 1133
Temperature 230 °C -
Load 2.16 kg -
ASTM Data
Melt Flow Index, MFI 2.1 g/10min ASTM D 1238
Temperature 230 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1400 MPa ISO 527
Yield stress 34 MPa ISO 527
Yield strain 11 % ISO 527
Strain at break >50 % ISO 527
Charpy notched impact strength, +23°C 8 kJ/m² ISO 179/1eA
Ball indentation hardness 70 MPa ISO 2039-1
ASTM Data
Tensile Strength at Yield 33 MPa ASTM D 638
Elongation at Yield 11 % ASTM D 638
Flexural Modulus 1450 MPa ASTM D 790
Izod Impact notched, 1/8 in 40 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 0.45 MPa 80 °C ISO 75-1/-2
Vicat softening temperature, A 150 °C ISO 306
ASTM Data
DTUL @ 66 psi 95 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 107 - ASTM D 2457
Haze 45 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 900 kg/m³ ISO 1183
Density 900 kg/m³ ASTM D 792
Characteristics
Processing
Profile Extrusion, Sheet Extrusion, Blow Molding, Thermoforming
Special Characteristics
Opaque
Features
Homopolymer
Applications
Packaging
Regional Availability
Asia Pacific, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.