Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIPLENE F30 AGR - PP-GF30 - Soredi S.p.a.

Material Data Center offers the following functions for NIPLENE F30 AGR:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Niplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 4 g/10min ASTM D 1238
Temperature 230 °C -
Load 2.16 kg -
Mold Shrinkage, MD 0.004 mm/mm ASTM D 955
Mold Shrinkage, TD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Break 90 MPa ASTM D 638
Flexural Modulus 6000 MPa ASTM D 790
Flexural Strength 140 MPa ASTM D 790
Rockwell Hardness R 113 - ASTM D 785
Izod Impact notched, 1/8 in 125 J/m ASTM D 256
Izod Impact notched, Low-Temperature 76.9 J/m ASTM D 256
Temperature -20 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Coeff. of linear therm. expansion, normal 30 E-6/K ISO 11359-1/-2
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 1.6 mm -
DTUL @ 264 psi 153 °C ASTM D 648
Vicat Temperature 144 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 2.7 - IEC 62631-2-1
Volume resistivity 1E13 Ohm*m IEC 62631-3-1
Surface resistivity 1E14 Ohm IEC 62631-3-2
Electric strength 60 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Humidity absorption 0.1 % Sim. to ISO 62
Density 1120 kg/m³ ASTM D 792
Characteristics
Features
Chemically Coupled Reinforcement, Homopolymer
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.