Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIRION 3550/M - PC - Soredi S.p.a.

Material Data Center offers the following functions for NIRION 3550/M:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Nirion datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 42.5 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mold Shrinkage, MD 0.0065 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Flexural Modulus 2400 MPa ASTM D 790
Flexural Strength 80 MPa ASTM D 790
Rockwell Hardness R 65 - ASTM D 785
Izod Impact notched, 1/8 in 432 J/m ASTM D 256
Izod Impact notched, Low-Temperature 48 J/m ASTM D 256
Temperature -20 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Coeff. of linear therm. expansion, normal 70 E-6/K ISO 11359-1/-2
ASTM Data
DTUL @ 264 psi 122 °C ASTM D 648
Vicat Temperature 143 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3 - IEC 62631-2-1
Dissipation factor, 1MHz 90 E-4 IEC 62631-2-1
Volume resistivity 1E12 Ohm*m IEC 62631-3-1
Surface resistivity 1E15 Ohm IEC 62631-3-2
Electric strength 25 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Water absorption 0.3 % Sim. to ISO 62
Humidity absorption 0.12 % Sim. to ISO 62
Density 1200 kg/m³ ASTM D 792
Characteristics
Processing
Injection Molding
Applications
General Purpose
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.