Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7115PF - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7115PF:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 14 cm³/10min ISO 1133
Temperature 260 °C -
Load 5 kg -
ASTM Data
Melt Flow Index, MFI 16 g/10min ASTM D 1238
Temperature 260 °C -
Load 5 kg -
Mold Shrinkage, MD 0.007 mm/mm ASTM D 955
Mold Shrinkage, TD 0.007 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1430 MPa ISO 527
Yield stress 30 MPa ISO 527
Strain at break 125 % ISO 527
Flexural modulus, 23°C 1440 MPa ISO 178
Flexural strength 46 MPa ISO 178
Izod notched impact strength 37 kJ/m² ISO 180/1A
Temperature 8 °C -
Tensile notched impact strength, +23°C -30 kJ/m² ISO 8256/1
ASTM Data
Tensile Modulus 1240 MPa ASTM D 638
Tensile Strength at Yield 35 MPa ASTM D 638
Tensile Strength at Break 34 MPa ASTM D 638
Elongation at Yield 8 % ASTM D 638
Elongation at Break 125 % ASTM D 638
Flexural Modulus 1370 MPa ASTM D 790
Flexural Strength 51 MPa ASTM D 790
Izod Impact notched, 1/8 in 534 J/m ASTM D 256
Izod Impact notched, 1/4 in 81 J/m ASTM D 256
Izod Impact notched, Low-Temperature -30 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 82 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 110 °C ISO 75-1/-2
Vicat softening temperature, A 131 °C ISO 306
ASTM Data
Coefficient of Thermal Expansion, MD 78 E-6/K ASTM D 696
Coefficient of Thermal Expansion, TD 130 E-6/K ASTM D 696
DTUL @ 66 psi 111 °C ASTM D 648
DTUL @ 264 psi 84 °C ASTM D 648
Vicat Temperature 83 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 990 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 60 - 65 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Mold temperature 30 - 50 °C -
Zone 1 225 - 275 °C -
Zone 2 240 - 280 °C -
Zone 3 250 - 290 °C -
Nozzle temperature 260 - 290 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Chemical Resistance
Hydrolytically Stable
Certifications
Food contact, Food approval FDA 21 CFR
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.