Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NOVADURAN 5510S - PBT - Mitsubishi Engineering-Plastics Corporation

Material Data Center offers the following functions for NOVADURAN 5510S:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Novaduran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 33 cm³/10min ISO 1133
Temperature 250 °C -
Load 2.16 kg -
Molding shrinkage, parallel 2.2 % ISO 294-4, 2577
Molding shrinkage, normal 2.0 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 420 MPa ISO 527
Yield stress 21 MPa ISO 527
Yield strain 21 % ISO 527
Strain at break 200 % ISO 527
Flexural modulus, 23°C 360 MPa ISO 178
Flexural strength 22 MPa ISO 178
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 30 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 219 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 74 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 139 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 150 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 150 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3.2 - IEC 62631-2-1
Dissipation factor, 1MHz 200 E-4 IEC 62631-2-1
Volume resistivity 1E14 Ohm*m IEC 62631-3-1
Surface resistivity 1E15 Ohm IEC 62631-3-2
Electric strength 22 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Water absorption 0.4 % Sim. to ISO 62
Density 1240 kg/m³ ISO 1183
Processing Recommendation ExtrusionValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 5 - 8 h -
Mold temperature 60 - 100 °C -
Zone 1 240 - 260 °C -
Zone 2 240 - 260 °C -
Zone 3 240 - 260 °C -
Nozzle temperature 260 °C -
Characteristics
Processing
Other Extrusion
Features
Copolymer, Impact Copolymer
Applications
Automotive, Electrical and Electronical, General Purpose
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.