Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® ECO P2H-AT MR50 - ABS - INEOS Styrolution

Material Data Center offers the following functions for Novodur® ECO P2H-AT MR50:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Novodur® ECO P2H-AT MR50 is a general purpose injection molding grade providing high flowability available in white colour. The product contains 50% post-consumer mechanically recyled ABS and has received RecyClass certification.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 38 % (ISO 14044)
Post-Consumer Recycled ABS Content (RecyClass-certified): 50 %
Colour: anthracite
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 33 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Molding shrinkage, parallel 0.6 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2500 MPa ISO 527
Yield stress 45 MPa ISO 527
Yield strain 2.2 % ISO 527
Nominal strain at break 6 % ISO 527
Flexural modulus, 23°C 2400 MPa ISO 178
Flexural strength 70 MPa ISO 178
Charpy impact strength, +23°C 80 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 70 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 18 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 8 kJ/m² ISO 179/1eA
Ball indentation hardness 85 MPa ISO 2039-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 91 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 95 °C ISO 75-1/-2
Vicat softening temperature, B 96 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.0 mm -
Yellow Card available yes - -
Other propertiesValueUnitTest Standard
Density 1050 kg/m³ ISO 1183
Recycled resin content 50 % -
Bulk density 600 kg/m³ -
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 230 - 260 °C -
Mold temperature 60 - 80 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets, White
Features
High Gloss
Certifications
Recycled Resin Content
Applications
Electrical and Electronical, General Purpose, Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 230 - 260°C

Mold temperature, range: 60 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.