Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® Ultra 4000PG - ABS - INEOS Styrolution

Material Data Center offers the following functions for Novodur® Ultra 4000PG:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Novodur® Ultra 4000PG acrylonitrile butadiene styrene (ABS) polymer features high surface quality and good impact strength. Novodur® Ultra 4000PG is an injection molding grade especially suitable for electroplating, providing enhanced heat resistance.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 7 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Thermal conductivity of melt 0.13 W/(m K) -
Spec. heat capacity of melt 1800 J/(kg K) -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2400 MPa ISO 527
Yield stress 46 MPa ISO 527
Yield strain 3.1 % ISO 527
Nominal strain at break 17 % ISO 527
Charpy notched impact strength, +23°C 23 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 98 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 103 °C ISO 75-1/-2
Vicat softening temperature, B 107 °C ISO 306
Coeff. of linear therm. expansion, parallel 90 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.0 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Electric strength 38 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1050 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Novodur® Ultra 4000PG, ABS, INEOS Styrolution
Shearstress-shear rate , Novodur® Ultra 4000PG, ABS, INEOS Styrolution
Stress-strain , Novodur® Ultra 4000PG, ABS, INEOS Styrolution
Secant modulus-strain , Novodur® Ultra 4000PG, ABS, INEOS Styrolution
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Platable
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 230 - 260°C

Mold temperature, range: 60 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.