Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® Ultra 4255 - (ABS+PC) - INEOS Styrolution

Material Data Center offers the following functions for Novodur® Ultra 4255:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Novodur® Ultra 4255 acrylonitrile butadiene styrene (ABS) polymer features high surface quality and good impact strength. Novodur® Ultra 4255 is PC modified injection molding grade combining very high impact strength at room as well as at low temperature, 100 % ductility at -30 °C, high heat resistance and a best in class flowability. Furthermore, it is of low emission, i.e. suitable to produce parts which fulfill interior emission requirements of the automotive OEMs.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 17 cm³/10min ISO 1133
Temperature 260 °C -
Load 5 kg -
Density of melt 966 kg/m³ -
Thermal conductivity of melt 0.211 W/(m K) -
Spec. heat capacity of melt 2250 J/(kg K) -
Ejection temperature 101 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2100 MPa ISO 527
Yield stress 47 MPa ISO 527
Yield strain 4.1 % ISO 527
Nominal strain at break >50 % ISO 527
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 55 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 55 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 103 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 116 °C ISO 75-1/-2
Vicat softening temperature, B 110 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.0 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Electric strength 35 kV/mm IEC 60243-1
Comparative tracking index 275 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1100 kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Features
Low Emission
Regional Availability
North America, Europe, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING

Pre-drying, Temperature: 80 - 90°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 250 - 270°C

Mold temperature, range: 60 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.