Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of P84®UHT 40G HCM - PI-CD - Evonik Operations GmbH

Material Data Center offers the following functions for P84®UHT 40G HCM:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other P84 datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

High temperature resistance, graphite filled (40%) Polyimide

Polyimid P84®UHT - at a glance

 

  • Excellent thermal-oxidative stability (use up to 300 ° C)
  • High mechanical strength and dimensional stability even at very high temperatures
  • Good creep resistance under load even at high temperatures
  • Easy machinability with standard tools for metals
  • Excellent tribological properties, high wear resistance
  • Processing by hot compression molding

 

 

Application examples

bushings, seals, bearings components, guides, gear wheels, and valve parts

in the automotive and aerospace industries and in industrial equipment.

For further information please visit WWW.P84.COM.

Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 8581 MPa ISO 527
Stress at break 77 MPa ISO 527
Strain at break 1.7 % ISO 527
Charpy impact strength, +23°C 7 kJ/m² ISO 179/1eU
Type of failure C - -
Charpy notched impact strength, +23°C 2 kJ/m² ISO 179/1eA
Type of failure C - -
Shore D hardness 84 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 0.45 MPa 364 °C ISO 75-1/-2
Other propertiesValueUnitTest Standard
Density 1670 kg/m³ ISO 1183
Characteristics
Processing
Compression Molding
Delivery form
Pellets, Granules, Powder
Additives
Lubricants
Special Characteristics
Increased electrical conductivity, Heat stabilized or stable to heat
Features
Creep Resistance, Thermal Stability, Tribologic Grade
Chemical Resistance
Oxidation Resistance
Applications
Aircraft and Aerospace, Automotive
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.