Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of P84®NT2 HCM - PI - Evonik Operations GmbH

Material Data Center offers the following functions for P84®NT2 HCM:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other P84 datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Neat aromatic Polyimide

Polyimid P84® NT - at a glance

 

  • Excellent performance at high temperatures
  • High strength and excellent shape stability
  • Very good impact resistance
  • High heat deflection temperature
  • Very good creep resistance even at elevated temperatures
  • Machinable with standard tools
  • Low wear and friction behaviour
  • Processing by Hot compression molding

 

 

Application examples

bushings, seals, bearings components, guides, gear wheels, and valve parts

in the automotive and aerospace industries and in industrial equipment.

For further information please visit WWW.P84.COM.

Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3428 MPa ISO 527
Stress at break 132 MPa ISO 527
Strain at break 6.3 % ISO 527
Charpy impact strength, +23°C 133 kJ/m² ISO 179/1eU
Type of failure C - -
Charpy notched impact strength, +23°C 7.5 kJ/m² ISO 179/1eA
Type of failure C - -
Shore D hardness 88 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 364 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 340 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 377 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 36 E-6/K ISO 11359-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Electric strength 37 kV/mm IEC 60243-1
Comparative tracking index 125 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1380 kg/m³ ISO 1183
Characteristics
Processing
Compression Molding
Delivery form
Pellets, Granules, Powder
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Features
Creep Resistance, Tribologic Grade
Applications
Aircraft and Aerospace, Automotive
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.