Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Panlite® ML-6500ZAH - PC - Teijin Chemicals Ltd.

Material Data Center offers the following functions for Panlite® ML-6500ZAH:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Panlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 2.5 cm³/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
Molding shrinkage, parallel 0.6 % ISO 294-4, 2577
Molding shrinkage, normal 0.6 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2400 MPa ISO 527
Yield stress 64 MPa ISO 527
Yield strain 6 % ISO 527
Nominal strain at break 30 % ISO 527
Stress at break 50 MPa ISO 527
Flexural modulus, 23°C 2140 MPa ISO 178
Flexural strength 98 MPa ISO 178
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 13 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 127 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 70 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 70 E-6/K ISO 11359-1/-2
Burning behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 0.8 mm -
Burning behav. 5V at thickness h 5VB class IEC 60695-11-20
Thickness tested 2.0 mm -
Glow Wire Flammability Index (GWFI) 930 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (2) 3 mm -
ASTM Data
UL 94 Flame rating V-0 - UL 94
Thickness tested 1 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Optical propertiesValueUnitTest Standard
ASTM Data
Light Transmittance 47 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ISO 1183
Processing Recommendation ExtrusionValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 5 - 8 h -
Melt temperature 270 - 320 °C -
Nozzle temperature 270 - 320 °C -
Characteristics
Processing
Other Extrusion
Delivery form
Pellets, White
Special Characteristics
Flame retardant, U.V. stabilized or stable to weather
Features
Light Diffusing
Applications
Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.