Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 2533 SD 02 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 2533 SD 02:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Polyether block amide Pebax® 2533 SD 02 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This SD grade is heat and UV stabilized and contains mould release additive.


Main applications:
  • Flexible injected parts
  • Silent gears


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 12 / 10 MPa ISO 527
Stress at 50% strain 3 / 3 MPa ISO 527
Strain at break >50 / >50 % ISO 527
Stress at 10% elongation 1 / * MPa ISO 527
Stress at 100% elongation 4 / * MPa ISO 527
Stress at break TPE 32 / * MPa ISO 527
Strain at break TPE >300 / * % ISO 527
Compression set at 23 °C, 24h 19 / * % ISO 815
Tear strength 44 / * kN/m ISO 34-1
Abrasion resistance 130 / * mm³ ISO 4649
Shore A hardness 74 / * - ISO 7619-1
Shore D hardness 22 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 134 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min -65 / * °C ISO 11357-1/-2
Temp. of deflection under load, 0.45 MPa 42 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 200 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Yellow Card available yes / * - -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 6 / - - IEC 62631-2-1
Relative permittivity, 1MHz 6 / - - IEC 62631-2-1
Dissipation factor, 100Hz 552 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 378 / - E-4 IEC 62631-2-1
Volume resistivity 1.3E10 / - Ohm*m IEC 62631-3-1
Surface resistivity * / 3E12 Ohm IEC 62631-3-2
Electric strength 36 / - kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.2 / * % Sim. to ISO 62
Humidity absorption 0.4 / * % Sim. to ISO 62
Density 1000 / 1000 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Pebax® 2533 SD 02, TPA, ARKEMA
Shearstress-shear rate , Pebax® 2533 SD 02, TPA, ARKEMA
Stress-strain , Pebax® 2533 SD 02 (dry), TPA, ARKEMA
Secant modulus-strain , Pebax® 2533 SD 02 (dry), TPA, ARKEMA
Stress-strain (isochronous) 23°C, Pebax® 2533 SD 02 (dry), TPA, ARKEMA
Creep modulus-time 23°C, Pebax® 2533 SD 02 (dry), TPA, ARKEMA
Creep curve 23°C, Pebax® 2533 SD 02 (dry), TPA, ARKEMA
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Other Extrusion, Transfer Molding, Casting, Thermoforming
Delivery form
Pellets
Additives
Lubricants, Antiblocking agent
Special Characteristics
Platable, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 180°C / 210°C / 240°C.
- Typical mold temperature : 10 – 30°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 55-65°C.

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.