Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 6333 SP 01 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 6333 SP 01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Polyether block amide Pebax® 6333 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This SP grade has been developed to be heat and UV resistant.


Main applications:
  • Athletic foot wear components
  • Ski boots


Packaging:

This grade is delivered dried in sealed packaging (20 or 25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 307 / 240 MPa ISO 527
Yield stress 19 / 18 MPa ISO 527
Yield strain 22 / 22 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy notched impact strength, -30°C - / 20 kJ/m² ISO 179/1eA
Stress at 10% elongation 14 / * MPa ISO 527
Stress at 100% elongation 17 / * MPa ISO 527
Stress at break TPE 53 / * MPa ISO 527
Strain at break TPE >300 / * % ISO 527
Compression set at 23 °C, 24h 47 / * % ISO 815
Tear strength 127 / * kN/m ISO 34-1
Abrasion resistance 55 / * mm³ ISO 4649
Shore D hardness 58 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 169 / * °C ISO 11357-1/-3
Temp. of deflection under load, 0.45 MPa 90 / * °C ISO 75-1/-2
Vicat softening temperature, B 85 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 140 / * E-6/K ISO 11359-1/-2
Oxygen index 20 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 9 / - - IEC 62631-2-1
Relative permittivity, 1MHz 4 / - - IEC 62631-2-1
Dissipation factor, 100Hz 1440 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 757 / - E-4 IEC 62631-2-1
Volume resistivity 9E11 / - Ohm*m IEC 62631-3-1
Surface resistivity * / 1E13 Ohm IEC 62631-3-2
Electric strength 42.5 / - kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.1 / * % Sim. to ISO 62
Humidity absorption 0.7 / * % Sim. to ISO 62
Density 1010 / 1010 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 65 - 75 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 230 - 290 °C -
Mold temperature 25 - 60 °C -
Diagrams
Viscosity-shear rate , Pebax® 6333 SP 01, TPA, ARKEMA
Shearstress-shear rate , Pebax® 6333 SP 01, TPA, ARKEMA
Dynamic Shear modulus-temperature , Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Stress-strain , Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Secant modulus-strain , Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Stress-strain (isochronous) 23°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Stress-strain (isochronous) 40°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Creep modulus-time 40°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Creep curve 40°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Stress-strain (isochronous) 60°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Creep modulus-time 60°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Creep curve 60°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Stress-strain (isochronous) 80°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Creep modulus-time 80°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Creep curve 80°C, Pebax® 6333 SP 01 (dry), TPA, ARKEMA
Specific volume-temperature (pvT) , Pebax® 6333 SP 01, TPA, ARKEMA
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Other Extrusion, Transfer Molding, Casting, Thermoforming
Delivery form
Pellets
Special Characteristics
Platable, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 260°C / 290°C.
- Typical mold temperature : 25 – 60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.
Other extrusion

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 225°C / 240°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.