Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® MV 1074 SP 01 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® MV 1074 SP 01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Polyether block amide Pebax® MV 1074 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
Pebax® MV 1074 SP 01 resin is an inherently dissipative polymer and can be dry blended or compounded with an isolative polymer to lower the surface resistivity. This hydrophilic grade when extruded into either a thin film or laminated on to a substrate offers excellent permeability to moisture vapor while remaining waterproof.
This SP grade has been developed to be heat and UV resistant.

Refractive index according to an internal method is 1.502.


Main applications:
  • Breathable membranes
  • Permanent antistactic additive


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 97 / 80 MPa ISO 527
Stress at 50% strain 10 / 10 MPa ISO 527
Strain at break >50 / >50 % ISO 527
Stress at break TPE 30 / * MPa ISO 527
Strain at break TPE >300 / * % ISO 527
Shore D hardness 38 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 158 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min -40 / * °C ISO 11357-1/-2
Oxygen index 19 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1.5E9 / 2.5E7 Ohm*m IEC 62631-3-1
Surface resistivity * / 3E9 Ohm IEC 62631-3-2
Electric strength 5 / - kV/mm IEC 60243-1
Other propertiesdry / condUnitTest Standard
Water absorption 48 / * % Sim. to ISO 62
Humidity absorption 1.4 / * % Sim. to ISO 62
Density 1070 / - kg/m³ ISO 1183
Film Propertiesdry / condUnitTest Standard
ISO Data
Maximum stress, parallel 32 / * MPa ISO 527-3
Maximum stress, normal 34 / * MPa ISO 527-3
Maximum strain, parallel 500 / * % ISO 527-3
Maximum strain, normal 700 / * % ISO 527-3
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 65 - 75 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 200 - 270 °C -
Mold temperature 25 - 60 °C -
Diagrams
Viscosity-shear rate , Pebax® MV 1074 SP 01, TPA, ARKEMA
Shearstress-shear rate , Pebax® MV 1074 SP 01, TPA, ARKEMA
Stress-strain , Pebax® MV 1074 SP 01 (dry), TPA, ARKEMA
Secant modulus-strain , Pebax® MV 1074 SP 01 (dry), TPA, ARKEMA
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Other Extrusion, Transfer Molding, Casting, Thermoforming
Delivery form
Pellets
Special Characteristics
Increased electrical conductivity, Anti-static, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 200°C / 240°C / 270°C.
- Typical mold temperature: 25–60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours): 4-6 hours at 65-75°C.
Other extrusion

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 210°C / 220°C / 230°C.
- Drying time and temperature (only necessary for bags opened for more than two hours): 4-6 hours at 65-75°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.