Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PHARMALENE® FF 55 PH BA - EVAC - Versalis S.p.A

Material Data Center offers the following functions for PHARMALENE® FF 55 PH BA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pharmalene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Pharmalene FF 55 PH BA will be bio attributed for 81%.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 0.7 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Shore A hardness 89 - ISO 7619-1
Shore D hardness 38 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 86 °C ISO 11357-1/-3
Vicat softening temperature, A 65 °C ISO 306
Optical propertiesValueUnitTest Standard
ISO Data
Haze 1.5 - ISO 14782
ASTM Data
Gloss 87 - ASTM D 2457
Other propertiesValueUnitTest Standard
Density 941 kg/m³ ISO 1183
Film PropertiesValueUnitTest Standard
ISO Data
Stress at yield, parallel 4 MPa ISO 527-3
Stress at yield, normal 4 MPa ISO 527-3
Stress at break, parallel 36 MPa ISO 527-3
Stress at break, normal 34 MPa ISO 527-3
Maximum strain, parallel 500 % ISO 527-3
Maximum strain, normal 700 % ISO 527-3
Dart drop A 700 g ISO 7765-1
Dynamic coefficient of friction 0.5 - ISO 8295
Type of extrusion blown - -
Processing Recommendation ExtrusionValueUnitTest Standard
Type of extrusion blown - -
Melt temperature 150 - 180 °C -
Characteristics
Processing
Blown Film Extrusion, Film Extrusion
Delivery form
Pellets
Special Characteristics
High impact or impact modified
Features
Copolymer
Certifications
Contains renewable resources, Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Medical Grade, US Pharmacopeia Class VI Approved, ISCC Plus
Applications
Medical, Packaging
Regional Availability
Europe, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.