Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PHARMALENE® FL 35 PH BCA - EVAC - Versalis S.p.A

Material Data Center offers the following functions for PHARMALENE® FL 35 PH BCA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pharmalene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Pharmalene FL 35 PH BCA will be bio attributed for 91%.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 2.5 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Flexural modulus, 23°C 90 MPa ISO 178
Shore A hardness 94 - ISO 7619-1
Shore D hardness 42 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 97 °C ISO 11357-1/-3
Vicat softening temperature, A 72 °C ISO 306
Optical propertiesValueUnitTest Standard
ISO Data
Haze 3 - ISO 14782
ASTM Data
Gloss 80 - ASTM D 2457
Other propertiesValueUnitTest Standard
Density 929 kg/m³ ISO 1183
Film PropertiesValueUnitTest Standard
ISO Data
Stress at yield, parallel 6 MPa ISO 527-3
Stress at yield, normal 6 MPa ISO 527-3
Stress at break, parallel 28 MPa ISO 527-3
Stress at break, normal 28 MPa ISO 527-3
Maximum strain, parallel 500 % ISO 527-3
Maximum strain, normal 700 % ISO 527-3
Dart drop A 450 g ISO 7765-1
Dynamic coefficient of friction 0.5 - ISO 8295
Type of extrusion blown - -
Processing Recommendation ExtrusionValueUnitTest Standard
Type of extrusion blown - -
Melt temperature 170 - 200 °C -
Characteristics
Processing
Injection Molding, Blown Film Extrusion, Film Extrusion, Other Extrusion
Delivery form
Pellets
Features
Heat Sealable, Copolymer
Certifications
Contains renewable resources, Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Medical Grade, US Pharmacopeia Class VI Approved, ISCC Plus
Applications
Medical
Regional Availability
Europe, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.