Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PHARMALENE® MP 20 PH BA - (PE-LD) - Versalis S.p.A

Material Data Center offers the following functions for PHARMALENE® MP 20 PH BA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pharmalene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Pharmalene MP 20 PH BA will be bio attributed for 100%.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 8 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 10 MPa ISO 527
Flexural modulus, 23°C 130 MPa ISO 178
Shore D hardness 48 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 108 °C ISO 11357-1/-3
Vicat softening temperature, A 88 °C ISO 306
Other propertiesValueUnitTest Standard
Density 921 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Mold temperature 10 - 30 °C -
Zone 1 160 - 200 °C -
Characteristics
Processing
Injection Molding, Coating
Delivery form
Pellets
Certifications
Contains renewable resources, Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Medical Grade, US Pharmacopeia Class VI Approved, ISCC Plus
Applications
Medical, Packaging
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.