Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Optical POQ64 - PMMA - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Optical POQ64:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Productprofil:

PLEXIGLAS® Optical POQ64 is an amorphous thermoplastic molding compound based on polymethyl methacrylate (PMMA).

 

In addition to the familiar properties of PLEXIGLAS® molding compounds, such as

 

  • excellent light transmission and brilliance,
  • good weather resistance,
  • high mechanical strength, surface hardness and mar resistance,

 

PLEXIGLAS® Optical POQ64 is distinguished by its

 

  • guaranteed purity and clarity,
  • very good flow properties,
  • optimised mold release behavior,
  • high luminous efficiency in medium to long light paths.

Application:

PLEXIGLAS® Optical POQ64 is excellently suited for the injection molding or injection-compression molding of technical components to meet stringent optical requirements.

Example:

Small to medium-sized injection-molded or injection compression-molded lightguide panels for display applications, lightguides.

Processing:

PLEXIGLAS® Optical POQ64 can be processed on injection molding machines with conventional three-section screws for engineering thermoplastics.

Physical Form / Packaging:

PLEXIGLAS® Optical POQ64 is supplied as uniform pellets in big-bags; other packaging on request.

Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 9 cm³/10min ISO 1133
Temperature 230 °C -
Load 3.8 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3300 MPa ISO 527
Stress at break 65 MPa ISO 527
Strain at break 3 % ISO 527
Charpy impact strength, +23°C 20 kJ/m² ISO 179/1eU
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 97 °C ISO 75-1/-2
Vicat softening temperature, B 104 °C ISO 306
Coeff. of linear therm. expansion, parallel 65 E-6/K ISO 11359-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Optical propertiesValueUnitTest Standard
ISO Data
Luminous transmittance 92 % ISO 13468-1, -2
Other propertiesValueUnitTest Standard
Density 1190 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Processing conditions acc. ISO 8257 - ISO ....-2
Injection Molding, mold temperature 64 °C ISO 294
Injection Molding, injection velocity 195 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 90 °C -
Pre-drying - Time 2 - 3 h -
Melt temperature 220 - 240 °C -
Mold temperature 60 - 90 °C -
Diagrams
Viscosity-shear rate , PLEXIGLAS® Optical POQ64, PMMA, Röhm
Shearstress-shear rate , PLEXIGLAS® Optical POQ64, PMMA, Röhm
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion, Other Extrusion, Compression Molding
Delivery form
Pellets
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Transparent
Features
Amorphous
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING
Predrying temperature: max. 90 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 240°C
Mold temperature:60 - 90°C
Profile extrusion
PREPROCESSING
Predrying temperature: max. 90 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 240 °C
Die temperature: 220 - 240 °C
Sheet extrusion
PREPROCESSING
Predrying temperature: max. 90 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 240 °C
Die temperature: 220 - 240 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.