Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of POLYFLAM® RABS 90000 UV5 - ABS - LyondellBasell Industries

Material Data Center offers the following functions for POLYFLAM® RABS 90000 UV5:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Polyflam datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Flame retardant ABS grade without PBDE; increased thermal stability

Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 30 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2200 MPa ISO 527
Yield stress 42 MPa ISO 527
Yield strain 3 % ISO 527
Nominal strain at break >50 % ISO 527
Charpy impact strength, +23°C 80 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 45 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 10 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 80 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 92 °C ISO 75-1/-2
Vicat softening temperature, B 96 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
Burning Behav. 5V at thickness h 5VA class IEC 60695-11-20
Thickness tested 4.0 mm -
Yellow Card available yes - -
Oxygen index 28 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Comparative tracking index 475 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 3 - 4 h -
Melt temperature 220 - 250 °C -
Mold temperature 40 - 60 °C -
Diagrams
Viscosity-shear rate , POLYFLAM® RABS 90000 UV5, ABS, LyondellBasell
Shearstress-shear rate , POLYFLAM® RABS 90000 UV5, ABS, LyondellBasell
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion, Thermoforming
Delivery form
Granules
Special Characteristics
Flame retardant, U.V. stabilized or stable to weather
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING; Pretreatment
Predrying: 3-4h / 80°C

PROCESSING ;Processing:

Melttemperature220 - 250°C
Mouldtemperature40 - 60°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.