Processing/Physical Characteristics | Value | Unit | Test Standard |
Other Standards[S] |
Melt flow index, MFI |
12 |
g/10min |
DIN 53735 |
Temperature |
220 |
°C |
- |
Load |
10 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Charpy notched impact strength, +23°C |
10 |
kJ/m² |
ISO 179/1eA |
Izod notched impact strength, +23°C |
17 |
kJ/m² |
ISO 180/1A |
Other Standards[S] |
Tensile Modulus |
2400 |
MPa |
DIN 53457 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Thermal properties | Value | Unit | Test Standard |
Other Standards[S] |
Vicat softening temperature, B |
95 |
°C |
DIN 53460 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard |
Other Standards[S] |
Density |
1060 |
kg/m³ |
DIN 53479 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Characteristics
Delivery form
Black
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.