Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of POLYREX PH-888G - PS - CHIMEI Corporation

Material Data Center offers the following functions for POLYREX PH-888G:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Polyrex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 4 cm³/10min ISO 1133
Temperature 200 °C -
Load 5 kg -
Molding shrinkage, parallel 0.6 % ISO 294-4, 2577
ASTM Data
Melt Flow Index, MFI 4 g/10min ASTM D 1238
Temperature 200 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 35 MPa ISO 527
Stress at break 28 MPa ISO 527
Flexural modulus, 23°C 2200 MPa ISO 178
Flexural strength 48 MPa ISO 178
Charpy notched impact strength, +23°C 10 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 5.5 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 11 kJ/m² ISO 180/1A
Izod notched impact strength 5 kJ/m² ISO 180/1A
Temperature -30 °C -
ASTM Data
Tensile Strength at Break 31.3 MPa ASTM D 638
Flexural Modulus 2068 MPa ASTM D 790
Flexural Strength 46 MPa ASTM D 790
Rockwell Hardness L 65 - ASTM D 785
Izod Impact notched, 1/8 in 92.9 J/m ASTM D 256
Izod Impact notched, 1/4 in 83.3 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 79 °C ISO 75-1/-2
Vicat softening temperature, A 102 °C ISO 306
Vicat softening temperature, B 92 °C ISO 306
Coeff. of linear therm. expansion, parallel 50 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 1.5 mm -
Vicat Temperature 102 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ASTM Data
Arc Resistance 90 s ASTM D 495
Other propertiesValueUnitTest Standard
Density 1030 kg/m³ ISO 1183
Density 1050 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 3 h -
Mold temperature 40 - 70 °C -
Feed temperature 160 - 180 °C -
Zone 1 190 - 210 °C -
Nozzle temperature 185 - 205 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Features
High Gloss
Applications
IT / Business Machine
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.