Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Prisma® 3410 - PP - Braskem

Material Data Center offers the following functions for Prisma® 3410:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Prisma datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 10 g/10min ISO 1133
Temperature 230 °C -
Load 2.16 kg -
ASTM Data
Melt Flow Index, MFI 10 g/10min ASTM D 1238
Temperature 230 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 29 MPa ISO 527
Yield strain 13 % ISO 527
Flexural modulus, 23°C 1050 MPa ISO 178
Izod notched impact strength, +23°C 3.5 kJ/m² ISO 180/1A
Izod notched impact strength 1.3 kJ/m² ISO 180/1A
Temperature -20 °C -
Rockwell hardness R 82 - ISO 2039-2
ASTM Data
Tensile Strength at Yield 30 MPa ASTM D 638
Elongation at Yield 13 % ASTM D 638
Rockwell Hardness R 83 - ASTM D 785
Izod Impact notched, 1/8 in 45 J/m ASTM D 256
Izod Impact notched, Low-Temperature 20 J/m ASTM D 256
Temperature -20 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 51 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 85 °C ISO 75-1/-2
Vicat softening temperature, A 129 °C ISO 306
ASTM Data
DTUL @ 66 psi 80 °C ASTM D 648
DTUL @ 264 psi 51 °C ASTM D 648
Vicat Temperature 129 °C ASTM D 1525
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 9 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 902 kg/m³ ASTM D 792
Characteristics
Processing
Injection Molding
Special Characteristics
Transparent
Features
Copolymer, Random Copolymer
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.