Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Promyde® B33 L - PA6 - Nurel S.A.

Material Data Center offers the following functions for Promyde® B33 L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Promyde datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 35 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 1.1 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 3300 / 1100 MPa ISO 527
Tensile Strength 85 / 40 MPa ISO 527
Yield strain 4 / 25 % ISO 527
Strain at break 50 / >50 % ISO 527
Flexural modulus, 23°C 2800 / 1000 MPa ISO 178
Charpy impact strength, +23°C N / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6 / 35 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 222 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 65 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 197 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 70 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 100 / * E-6/K ISO 11359-1/-2
ASTM Data
UL 94 Flame rating V-2 - UL 94
Thickness tested 1.5 mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3.5 / 7 - IEC 62631-2-1
Dissipation factor, 1MHz 230 / 3000 E-4 IEC 62631-2-1
Volume resistivity 1E13 / 1E10 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E10 Ohm IEC 62631-3-2
Comparative tracking index 600 / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 9.5 / * % Sim. to ISO 62
Humidity absorption 3 / * % Sim. to ISO 62
Density 1130 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 203 / * cm³/g ISO 307, 1157, 1628
Characteristics
Processing
Injection Molding, Other Extrusion
Additives
Lubricants, Release agent
Applications
Automotive, Electrical and Electronical
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.