Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Promyde® B300 P2 G30 S - PA6-GF30 - Nurel S.A.

Material Data Center offers the following functions for Promyde® B300 P2 G30 S:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Promyde datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 90 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 9900 / 6700 MPa ISO 527
Tensile Strength 195 / 115 MPa ISO 527
Strain at break 3 / 5 % ISO 527
Flexural modulus, 23°C 8400 / 5200 MPa ISO 178
Flexural strength 275 / 180 MPa ISO 178
Charpy impact strength, +23°C 85 / 95 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 75 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 13 / 25 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 222 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 210 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 215 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 20 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 60 / * E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.5 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Comparative tracking index 500 / - - IEC 60112
Other Standards[S]
Relative permittivity, 1MHz 3.8 / 6.8 - IEC 60250
Dissipation factor, 1MHz 230 / 2200 E-4 IEC 60250
Volume resistivity 1E13 / 1E10 Ohm*m IEC 60093
Surface resistivity * / 1E10 Ohm IEC 60093
S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesdry / condUnitTest Standard
Water absorption 6.7 / * % Sim. to ISO 62
Humidity absorption 2.1 / * % Sim. to ISO 62
Density 1360 / - kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature <80 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 235 - 250 °C -
Mold temperature 40 - 80 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Applications
Automotive, Electrical and Electronical
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.