Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Promyde® BF940L - PA* - Nurel S.A.

Material Data Center offers the following functions for Promyde® BF940L:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Promyde datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 18 cm³/10min ISO 1133
Temperature 275 °C -
Load 5 kg -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 200 °C ISO 11357-1/-3
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 0.5 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1110 kg/m³ ISO 1183
Moisture Content 0.1 % -
Film PropertiesValueUnitTest Standard
ISO Data
Stress at break, parallel 65 MPa ISO 527-3
Maximum strain, parallel 400 % ISO 527-3
Trouser Tear resistance, parallel 30 N/mm ISO 6383-1
Dynamic coefficient of friction 0.25 - ISO 8295
WVTR, 23°C/85%r.h. 20 g/(m²*d) ISO 15106-1/-2
Oxygen transmission rate, 23°C/0%r.h. 25 cm³/(m²*d*bar) ISO 15105-1/-2
Oxygen transmission rate, 23°C/85%r.h. 25 cm³/(m²*d*bar) ISO 15105-1/-2
Material specific propertiesValueUnitTest Standard
ISO Data
Viscosity number 263 cm³/g ISO 307, 1157, 1628
Processing Recommendation ExtrusionValueUnitTest Standard
Pre-drying - Temperature 75 - 80 °C -
Feed temperature 40 - 50 °C -
Zone 1 210 - 250 °C -
Nozzle temperature 240 - 250 °C -
Characteristics
Processing
Blown Film Extrusion, Film Extrusion, Thermoforming
Additives
Lubricants
Special Characteristics
Transparent
Certifications
Food contact
Applications
Packaging
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com