Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Provista™ MP001 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Provista™ MP001:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Provista datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Provista™ Copolymer MP001 is a resin specifically developed for extrusion into profiles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to commonly used materials, Eastman Provista™ copolymer runs on most standard processing equipment at increased speeds. An extremely high melt strength makes the resin an excellent choice when extruding profiles into complicated shapes. In addition to profile extrusion, Eastman Provista™ copolymer is an excellent choice for extrusion of rigid tubing. This product meets the biocompatibility requirements under FDA/ISO 10993 and USP Class 6, Plastics.




Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 50 MPa ASTM D 638
Tensile Strength at Break 29 MPa ASTM D 638
Elongation at Yield 4 % ASTM D 638
Elongation at Break 109 % ASTM D 638
Flexural Modulus 2200 MPa ASTM D 790
Flexural Strength 72 MPa ASTM D 790
Rockwell Hardness R 106 - ASTM D 785
Izod Impact notched, 1/8 in 94 J/m ASTM D 256
Izod Impact notched, Low-Temperature 52 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 67 °C ASTM D 648
DTUL @ 264 psi 62 °C ASTM D 648
Vicat Temperature 79 °C ASTM D 1525
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 171 - ASTM D 2457
Haze 0.6 % ASTM D 1003
Light Transmittance 90 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1270 kg/m³ ASTM D 792
Color b 0.61 - CIE
Characteristics
Processing
Pipe/Tube Extrusion, Profile Extrusion
Special Characteristics
Transparent
Features
High Gloss, Melt Strength, Copolymer
Certifications
Food contact, Food approval FDA 21 CFR, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.