Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pyramid™ KD2000-J02 - PEEK - Polymics, Ltd.

Material Data Center offers the following functions for Pyramid™ KD2000-J02:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pyramid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 20 g/10min ASTM D 1238
Mold Shrinkage, MD 0.012 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 3500 MPa ASTM D 638
Tensile Strength at Break 97 MPa ASTM D 638
Elongation at Break 30 % ASTM D 638
Compressive Strength 124 MPa ASTM D 695
Flexural Modulus 3500 MPa ASTM D 790
Rockwell Hardness M 102 - ASTM D 785
Shore D Hardness 88 - ASTM D 2240
Izod Impact notched, 1/8 in 80 J/m ASTM D 256
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
UL 94 Flame rating V-0 - UL 94
Coefficient of Thermal Expansion, MD 47 E-6/K ASTM D 696
DTUL @ 264 psi 160 °C ASTM D 648
Melting Temperature 339 °C ASTM D 3418
Glass Transition Temperature 143 °C ASTM E 1356
Thermal Conductivity, solid state 0.036 W/(m K) ASTM C 177
Electrical propertiesValueUnitTest Standard
ASTM Data
Dielectric Strength, Short Time 18 kV/mm ASTM D 149
Volume Resistivity 1E16 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Water Absorption, 24hr 0.2 % ASTM D 570
Density 1300 kg/m³ ASTM D 792
Characteristics
Delivery form
Pellets
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.