Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Radiflam A - PA66 - Radici Novacips SpA

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Radiflam A" in Material Data Center leads to the following information:

Tradename: Radiflam A
Family: PA66
Producer: Radici Novacips SpA
20 hits in the material database
2 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
RADIFLAM A FR 100 NT PA66
RADIFLAM A RV250 AF 375 BK PA66-GF25
RADIFLAM A RV250 FR 100 NT PA66-GF25
RADIFLAM A RV250 HF 333 BK PA66-GF25
RADIFLAM A RV250K AE 121 C NT PA66-GF25
RADIFLAM A RV300 AE 100 C NT PA66-GF30
RADIFLAM A RV350 HF 100 NT PA66-GF35
RADIFLAM A RV500 AF 821 BR PA66-GF50
RADIFLAM AESTUS T2 RV300 HF 100 NT PA6T/66-GF30
RADIFLAM A FR 122 NT PA66
RADIFLAM A FRX 308 BK PA66
RADIFLAM A FR 308 BK PA66
RADIFLAM A FR 5138 OR PA66
RADIFLAM A FRX 328 BK PA66
RADIFLAM A RV200 HF 100 NT PA66-GF20
RADIFLAM A RV250 HF 100 NT PA66-GF25
RADIFLAM A RV300 AF 830 BR PA66-GF30
RADIFLAM A RV300 HF 9293 GY PA66-GF30
RADIFLAM A RV350 AF 375 BK PA66-GF35
RADIFLAM AESTUS T2 RV300 HF 333 BK PA6T/66-GF30

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.