Material datasheets available free. Online registration at: www.materialdatacenter.com
Radilon DT - PA612 - RadiciGroup High Performance Polymers
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Radilon DT" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
RADILON DT 22D 1000 NT | PA612 |
RADILON DT 40E50USR 333C BK | PA612 |
RADILON DT HSW 105 M NT | PA612 |
RADILON DT RV300RKC2 306 BK | PA612-GF30 |
RADILON DT RV500RKC2 306 BK | PA612-GF50 |
RADILON DT RV300RKC2 106 NT | PA612-GF30 |
RADILON DT RV450USR 333 BK | PA612-GF45 |
RADILON DT RV500RKC2 106 NT | PA612-GF50 |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.