Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RamOfin PPH343T4BK10-1 - PP-T20 - Polyram

Material Data Center offers the following functions for RamOfin PPH343T4BK10-1:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ramofin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 10 g/10min ISO 1133
Temperature 230 °C -
Load 2.16 kg -
Other Standards[S]
Molding shrinkage, parallel 0.9 % Producer Method
Molding shrinkage, normal 1.1 % Producer Method
S: These properties are reported by the producer according standards that are different to our defaults.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2400 MPa ISO 527
Tensile Strength 33 MPa ISO 527
Yield strain 5 % ISO 527
Flexural modulus, 23°C 2300 MPa ISO 178
Flexural strength 50 MPa ISO 178
Charpy impact strength, +23°C 35 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 14 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 3 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 1.5 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 3 kJ/m² ISO 180/1A
Izod notched impact strength 2 kJ/m² ISO 180/1A
Temperature -30 °C -
ASTM Data
Izod Impact notched, 1/8 in 24 J/m ASTM D 256
Izod Impact notched, Low-Temperature 22 J/m ASTM D 256
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 163 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 70 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 110 °C ISO 75-1/-2
Burning behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.0 mm -
Burning rate, FMVSS, Thickness 1 mm 100 mm/min ISO 3795 (FMVSS 302)
Other propertiesValueUnitTest Standard
Density 1060 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.1 % -
Mold temperature 30 - 70 °C -
Feed temperature 60 - 70 °C -
Zone 1 200 - 230 °C -
Zone 2 200 - 230 °C -
Zone 3 200 - 250 °C -
Characteristics
Processing
Injection Molding
Delivery form
Black
Special Characteristics
Heat stabilized or stable to heat
Features
Homopolymer
Certifications
RoHS compliant
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.