Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt flow index, MFI |
6 |
g/10min |
ISO 1133 |
Temperature |
230 |
°C |
- |
Load |
2.16 |
kg |
- |
Other Standards[S] |
Molding shrinkage, parallel |
0.3 |
% |
Producer Method |
Molding shrinkage, normal |
0.8 |
% |
Producer Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Tensile Modulus |
6300 |
MPa |
ISO 527 |
Tensile Strength |
80 |
MPa |
ISO 527 |
Strain at break |
4 |
% |
ISO 527 |
Flexural modulus, 23°C |
5800 |
MPa |
ISO 178 |
Flexural strength |
151 |
MPa |
ISO 178 |
Charpy impact strength, +23°C |
46 |
kJ/m² |
ISO 179/1eU |
Charpy impact strength, -30°C |
44 |
kJ/m² |
ISO 179/1eU |
Charpy notched impact strength, +23°C |
9.5 |
kJ/m² |
ISO 179/1eA |
Charpy notched impact strength, -30°C |
7.5 |
kJ/m² |
ISO 179/1eA |
Izod notched impact strength, +23°C |
10.5 |
kJ/m² |
ISO 180/1A |
Izod notched impact strength |
8.5 |
kJ/m² |
ISO 180/1A |
Temperature |
-30 |
°C |
- |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Temp. of deflection under load, 1.80 MPa |
140 |
°C |
ISO 75-1/-2 |
Temp. of deflection under load, 0.45 MPa |
155 |
°C |
ISO 75-1/-2 |
Burning rate, FMVSS, Thickness 1 mm |
80 |
mm/min |
ISO 3795 (FMVSS 302) |
Electrical properties | Value | Unit | Test Standard |
Other Standards[S] |
Surface resistivity |
12 |
Ohm |
DIN 53482 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard |
Density |
1140 |
kg/m³ |
ISO 1183 |
Processing Recommendation Injection Molding | Value | Unit | Test Standard |
Pre-drying - Temperature |
80 |
°C |
- |
Pre-drying - Time |
2 - 4 |
h |
- |
Processing humidity |
≤0.1 |
% |
- |
Mold temperature |
30 - 70 |
°C |
- |
Feed temperature |
60 - 70 |
°C |
- |
Zone 1 |
200 - 230 |
°C |
- |
Zone 2 |
200 - 230 |
°C |
- |
Zone 3 |
200 - 250 |
°C |
- |
Characteristics
Processing
Injection Molding
Delivery form
Black
Special Characteristics
U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Features
Homopolymer
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com