Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RANPELEN SFC-750D - PP - Lotte Chemical Corporation

Material Data Center offers the following functions for RANPELEN SFC-750D:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ranpelen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 8 g/10min ISO 1133
ASTM Data
Melt Flow Index, MFI 7 g/10min ASTM D 1238
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 22 MPa ISO 527
Strain at break 500 % ISO 527
Flexural modulus, 23°C 784 MPa ISO 178
Rockwell hardness R 82 - ISO 2039-2
ASTM Data
Tensile Strength at Yield 21 MPa ASTM D 638
Elongation at Break 500 % ASTM D 638
Flexural Modulus 735 MPa ASTM D 790
Rockwell Hardness R 80 - ASTM D 785
Izod Impact notched, 1/8 in 78 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 132 °C ISO 11357-1/-3
Temp. of deflection under load, 0.45 MPa 70 °C ISO 75-1/-2
ASTM Data
DTUL @ 66 psi 70 °C ASTM D 648
Melting Temperature 130 °C ASTM D 3418
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 2 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 900 kg/m³ ISO 1183
Density 900 kg/m³ ASTM D 792
Characteristics
Processing
Film Extrusion
Special Characteristics
Transparent
Features
Heat Sealable, Copolymer, Random Copolymer
Certifications
Medical Grade, US Pharmacopeia Class VI Approved
Applications
Medical, Packaging
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.