Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AESNO P302 TL - PA12-I - ARKEMA

Material Data Center offers the following functions for Rilsamid® AESNO P302 TL:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
ISO 16396 - PA12-HIP, EGHL, C22-004

Rilsamid® AESNO P302 TL resin is a natural polyamide. 
This grade is plasticized and designed for tube extrusion.

Rilsamid® AESNO P302 TL resin falls into the PA12-HIPHL category according to DIN 73378.


Main applications:

Air brake. 
Tubing for use in motor vehicles

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. for any use above this limit, please refer to our technical services.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 13 / * cm³/10min ISO 1133
Temperature 235 / * °C -
Load 5 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 475 / 430 MPa ISO 527
Yield stress 28 / 24 MPa ISO 527
Yield strain 24 / 24 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy notched impact strength, +23°C 46 / - kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 4 / 6 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 174 / * °C ISO 11357-1/-3
Coeff. of linear therm. expansion, parallel 150 / * E-6/K ISO 11359-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E12 / 1E12 Ohm*m IEC 62631-3-1
Surface resistivity * / 7E13 Ohm IEC 62631-3-2
Electric strength 41 / 41 kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.2 / * % Sim. to ISO 62
Density 1030 / 1030 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Shearstress-shear rate , Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Dynamic Shear modulus-temperature , Rilsamid® AESNO P302 TL (dry), PA12-I, ARKEMA
Stress-strain , Rilsamid® AESNO P302 TL (dry), PA12-I, ARKEMA
Secant modulus-strain , Rilsamid® AESNO P302 TL (dry), PA12-I, ARKEMA
Stress-strain (isochronous) 23°C, Rilsamid® AESNO P302 TL (dry), PA12-I, ARKEMA
Creep modulus-time 23°C, Rilsamid® AESNO P302 TL (dry), PA12-I, ARKEMA
Creep curve 23°C, Rilsamid® AESNO P302 TL (dry), PA12-I, ARKEMA
LTHA-Strain at Break 2mm, Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
Characteristics
Processing
Injection Molding, Profile Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Lubricants, Plasticizer
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Profile extrusion

Processing conditions, Extrusion :

- Typical melt temperature (Min / Recommended / Max) : 200°C / 220°C / 240°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80°C.

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.