Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® ASR 13 - PA12-CF15 - ARKEMA

Material Data Center offers the following functions for Rilsamid® ASR 13:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
ISO 16396 - PA12, CF15M1GHL, C16-080

Rilsamid® ASR 13 resin is a carbon fiber reinforced polyamide. 
This black colored grade is designed for injection moulding.


Packaging : 
This grade is delivered dried in sealed packaging (25 kg bags / 450 kg rigid containers) ready to be processed

Shelf life : 
Two years from the delivery.
For any use above this limit please refer to our technical services. 
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 10 / * cm³/10min ISO 1133
Temperature 235 / * °C -
Load 5 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 9600 / 9000 MPa ISO 527
Stress at break 127 / 115 MPa ISO 527
Strain at break 3.3 / 4 % ISO 527
Charpy impact strength, +23°C 45 / 46 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 47 / 48 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 11 / 11 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 8 / 7 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 178 / * °C ISO 11357-1/-3
Electrical propertiesdry / condUnitTest Standard
ISO Data
Surface resistivity * / 100000 Ohm IEC 62631-3-2
Other propertiesdry / condUnitTest Standard
Water absorption 1.5 / * % Sim. to ISO 62
Humidity absorption 0.6 / * % Sim. to ISO 62
Density 1080 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Increased electrical conductivity, Anti-static, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 240°C / 260°C / 280°C.
- Typical mold temperature : 40 – 90°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.


Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.