Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AMNO P20 TLD - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AMNO P20 TLD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
PA12-P, MHLR, 12-005
Rilsamid® AMNO P20 TLD resin is a natural polyamide. This grade is plasticized and designed for injection molding.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 44 / * cm³/10min ISO 1133
Temperature 235 / * °C -
Load 2.16 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 620 / 550 MPa ISO 527
Yield stress 31 / 30 MPa ISO 527
Yield strain 20 / 20 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy notched impact strength, +23°C 9 / 14 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 3 / 3 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 173 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 48 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 130 / * °C ISO 75-1/-2
Vicat softening temperature, B 134 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 120 / * E-6/K ISO 11359-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz 8 / - - IEC 62631-2-1
Relative permittivity, 1MHz 4 / - - IEC 62631-2-1
Dissipation factor, 100Hz 2010 / - E-4 IEC 62631-2-1
Dissipation factor, 1MHz 595 / - E-4 IEC 62631-2-1
Volume resistivity - / 1E10 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E12 Ohm IEC 62631-3-2
Electric strength - / 26 kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.4 / * % Sim. to ISO 62
Density 1020 / 1020 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Rilsamid® AMNO P20 TLD, PA12, ARKEMA
Shearstress-shear rate , Rilsamid® AMNO P20 TLD, PA12, ARKEMA
Dynamic Shear modulus-temperature , Rilsamid® AMNO P20 TLD (dry), PA12, ARKEMA
Stress-strain , Rilsamid® AMNO P20 TLD (dry), PA12, ARKEMA
Secant modulus-strain , Rilsamid® AMNO P20 TLD (dry), PA12, ARKEMA
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent, Plasticizer
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding

Processing conditions, Injection:

- Typical melt temperature (Min / Recommended / Max) : 250°C / 270°C / 290°C.
- Mold temperature : 20 - 40°C
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80 - 90°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com