Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AMVO TLD - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AMVO TLD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
PA12, MHLR, 16-010
Rilsamid® AMVO TLD resin is a natural polyamide. This grade is designed for injection moulding.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 18 / * cm³/10min ISO 1133
Temperature 235 / * °C -
Load 2.16 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 1400 / 1260 MPa ISO 527
Yield stress 44 / 42 MPa ISO 527
Yield strain 7 / 7 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy notched impact strength, +23°C 5 / 5 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 5 / 6 kJ/m² ISO 179/1eA
Shore D hardness 72 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 55 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 135 / * °C ISO 75-1/-2
Vicat softening temperature, B 142 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 100 / * E-6/K ISO 11359-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity - / 1E12 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E14 Ohm IEC 62631-3-2
Electric strength - / 30 kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.6 / * % Sim. to ISO 62
Density 1010 / 1010 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Rilsamid® AMVO TLD, PA12, ARKEMA
Shearstress-shear rate , Rilsamid® AMVO TLD, PA12, ARKEMA
Stress-strain , Rilsamid® AMVO TLD (dry), PA12, ARKEMA
Secant modulus-strain , Rilsamid® AMVO TLD (dry), PA12, ARKEMA
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.