Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BESNO P20 TLO - PA11 - ARKEMA

Material Data Center offers the following functions for Rilsan® BESNO P20 TLO:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
PA11-P, EHL, 22-005
Rilsan® BESNO P20 TLO resin is a polyamide 11 produced from a renewable source. This natural grade is plasticized and designed for extrusion.

This grade contains a low amount of oligomers.




Main applications:
  • Fluid transportation
  • Tubing for use in motor vehicle
  • Clean hose for offshore umbilicals
  • Liner for steel pipes or composite tubes


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 2 / * cm³/10min ISO 1133
Temperature 235 / * °C -
Load 5 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus - / 510 MPa ISO 527
Yield stress - / 29 MPa ISO 527
Yield strain - / 39 % ISO 527
Nominal strain at break - / >50 % ISO 527
Charpy notched impact strength, -30°C - / 10 kJ/m² ISO 179/1eA
Shore D hardness 63 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 182 / * °C ISO 11357-1/-3
Other propertiesdry / condUnitTest Standard
Water absorption 1.8 / * % Sim. to ISO 62
Density 1040 / 1040 kg/m³ ISO 1183
Biobased content 93 % -
Diagrams
Viscosity-shear rate , Rilsan® BESNO P20 TLO, PA11, ARKEMA
Shearstress-shear rate , Rilsan® BESNO P20 TLO, PA11, ARKEMA
Dynamic Shear modulus-temperature , Rilsan® BESNO P20 TLO (dry), PA11, ARKEMA
Stress-strain , Rilsan® BESNO P20 TLO (dry), PA11, ARKEMA
Secant modulus-strain , Rilsan® BESNO P20 TLO (dry), PA11, ARKEMA
Stress-strain (isochronous) 40°C, Rilsan® BESNO P20 TLO (dry), PA11, ARKEMA
Creep modulus-time 40°C, Rilsan® BESNO P20 TLO (dry), PA11, ARKEMA
Creep curve 40°C, Rilsan® BESNO P20 TLO (dry), PA11, ARKEMA
Characteristics
Processing
Profile Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Lubricants, Plasticizer
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Certifications
Contains renewable resources
Regional Availability
Other text information
Other extrusion

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.
 - Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.


Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.