Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SCHULAMID® 6 GF 15 H - PA6-GF15 - LyondellBasell Industries

Material Data Center offers the following functions for SCHULAMID® 6 GF 15 H:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Schulamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.4 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.2 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 5800 / 3000 MPa ISO 527
Stress at break 120 / 70 MPa ISO 527
Strain at break 3.5 / 15 % ISO 527
Flexural modulus, 23°C 4300 / - MPa ISO 178
Flexural strength 170 / - MPa ISO 178
Charpy impact strength, +23°C 45 / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 40 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 7 / 15 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 5 / - kJ/m² ISO 179/1eA
Ball indentation hardness 174 / - MPa ISO 2039-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 200 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 210 / * °C ISO 75-1/-2
Vicat softening temperature, A 215 / * °C ISO 306
Vicat softening temperature, B 210 / * °C ISO 306
Burning behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.5 / * mm -
Burning behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Burning rate, FMVSS, Thickness 1 mm 43 mm/min ISO 3795 (FMVSS 302)
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (1) 1.5 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (1) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (2) 3 mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E13 / 1E10 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E12 Ohm IEC 62631-3-2
Other propertiesdry / condUnitTest Standard
Density 1230 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 145 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.1 % -
Melt temperature 250 - 280 °C -
Mold temperature 60 - 100 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
Heat stabilized or stable to heat
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.