Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SCHULAMID® 6 GF 15 HI - PA6-I-GF15 - LyondellBasell Industries

Material Data Center offers the following functions for SCHULAMID® 6 GF 15 HI:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Schulamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
15% glass fibre reinforced impact modified PA 6

Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.004 mm/mm ASTM D 955
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 5000 / 2600 MPa ISO 527
Stress at break 100 / 60 MPa ISO 527
Strain at break 5 / 15 % ISO 527
Charpy impact strength, +23°C 70 / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 56 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 16 / 24 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 7 / - kJ/m² ISO 179/1eA
ASTM Data
Tensile Strength at Break 91 / - MPa ASTM D 638
Elongation at Break 5 / - % ASTM D 638
Flexural Modulus 4068 / - MPa ASTM D 790
Flexural Strength 138 / - MPa ASTM D 790
Izod Impact notched, 1/8 in 171 / - J/m ASTM D 256
Thermal propertiesdry / condUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 190 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 210 / * °C ISO 75-1/-2
Vicat softening temperature, B 205 / * °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.5 / * mm -
Yellow Card available yes / * - -
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 3.0 / * mm -
Yellow Card available yes / * - -
Burning rate, FMVSS, Thickness 1 mm 100 mm/min ISO 3795 (FMVSS 302)
ASTM Data
DTUL @ 66 psi 221 °C ASTM D 648
DTUL @ 264 psi 204 °C ASTM D 648
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity >1E13 / - Ohm*m IEC 62631-3-1
Surface resistivity * / >1E15 Ohm IEC 62631-3-2
Other propertiesdry / condUnitTest Standard
Density 1200 / - kg/m³ ISO 1183
Density 1200 kg/m³ ASTM D 792
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 145 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 250 - 280 °C -
Mold temperature 60 - 90 °C -
Diagrams
Viscosity-shear rate , SCHULAMID® 6 GF 15 HI, PA6-I-GF15, LyondellBasell
Shearstress-shear rate , SCHULAMID® 6 GF 15 HI, PA6-I-GF15, LyondellBasell
Characteristics
Processing
Injection Molding
Delivery form
Granules
Additives
Release agent, Plasticizer
Special Characteristics
High impact or impact modified
Regional Availability
Other text information
Injection molding
PREPROCESSING; Pretreatment
Predrying: 4-6h / 80°C

PROCESSING ;Processing:

Melttemperature250 - 280°C
Mouldtemperature60 - 90°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.